Peracetic acid dissolves copper, brass, and carbon steel, and can corrode certain stainless steels under aggressive conditions. Its oxidative nature targets metals with weak or unstable passive layers, especially when heat, concentration, or contaminants like chlorides are present.
Metals that corrode in peracetic acid
Copper and brass
Peracetic acid rapidly attacks copper and brass, even in dilute solutions. The metal oxidizes to copper ions, which leach into the solution, causing visible blue-green staining and pitting. This reaction poses contamination risks in food and pharmaceutical systems, leading to equipment failure and product recalls.
Carbon steel
Carbon steel lacks a protective oxide layer and corrodes quickly in peracetic acid. The acid accelerates rust formation, leading to flaking and perforation within days. Even low concentrations and ambient temperatures cause significant material loss, making carbon steel unsuitable for any prolonged exposure.
Stainless steels: limited resistance under stress
304 and 316 stainless steel
Stainless steels 304 and 316 resist dilute, cool peracetic acid for short periods. However, above 40°C or at concentrations over 15%, the protective chromium oxide layer can break down. Chlorides in water dramatically increase the risk of pitting and stress corrosion cracking, even in 316 stainless with molybdenum.
Failures have been reported in industrial systems after months of use, particularly in food processing and wastewater applications where temperature and water quality vary.
Higher-grade stainless alloys
Duplex 2205 and super austenitic steels like 6% molybdenum alloys offer better resistance. Their enhanced chromium, molybdenum, and nitrogen content stabilizes the passive layer under harsh conditions. These materials are used in critical systems where long-term reliability justifies higher cost.
Metals that resist peracetic acid
Titanium
Titanium is highly resistant to peracetic acid, even at high concentrations and temperatures. Its stable oxide layer prevents corrosion in most environments. However, if connected to less noble metals in a system, it can drive galvanic corrosion of those materials.
Aluminum
Aluminum resists peracetic acid only under mild conditions—neutral pH and temperatures below 50°C. In acidic or hot solutions, the oxide layer dissolves, leading to pitting and hydrogen gas formation. This poses safety risks in enclosed systems and limits aluminum’s use in aggressive applications.
Nickel-based alloys
Alloys like Hastelloy C-276 and Inconel 625 show excellent resistance to peracetic acid, even in boiling, concentrated solutions. They are typically reserved for high-purity or critical processes where contamination or failure is unacceptable, due to their high cost.